1. Surface treatment: Make the conveyor belt joint into a beveled stepped joint according to the lap length of 1/2 of the bandwidth, then roughen the surface of the joint, and use cleaning agent to clean, decontaminate and dry it.
2. Apply glue: Apply vulcanized glue evenly once or twice on the surface of the joint and the vulcanized rubber sheet. Wait until the solution evaporates until the rubber surface is basically dry. Then attach the vulcanized rubber sheet to the surface of the joint coated with vulcanized glue and place it on the same cloth. Attach buffer strips to the gaps between layers (note that if the glue is not completely dry, bubbles will be generated, which will reduce the pinching performance).
3. Laminating and pressing: After the glue solvent evaporates until the glue surface is basically dry, laminate the two ends. When laminating, laminate from the middle to both sides of the conveyor belt (to facilitate the escape of air from both sides), and make sure the looseness of both sides of the film is consistent, the steps of each joint are aligned, and the center line is aligned. After bonding, roll it fully to prevent the accumulation of air bubbles, and press the two heating plates up and down the joint to apply a certain amount of pressure. When applying pressure, be careful not to dislocate the joints and the pressure should be uniform.
4. Heating and vulcanization: Install the vulcanization device. Increase the temperature and pressure. When the heating plate is heated for 15-25 minutes, press it once to ensure that the joint is under sufficient pressure. When the temperature reaches 80℃, the pressure is required to reach 1.0-2.0MPa, then stop pressurizing and continue heating. Start timing when the temperature rises to 145°C. The constant temperature is between 145°C and 150°C. After 45 minutes, stop heating immediately and allow it to cool naturally to normal temperature.
5. Trim. After the joint returns to normal temperature, remove the heating plate and cut off the overflowing residual glue and the rubber above the belt surface to make the joint surface flat, smooth and clean.